Hertzian indentation testing of glass-ionomer restoratives: A reliable and clinically relevant testing approach

Publication date: Available online 12 April 2013Source:Journal of Dentistry Objectives To investigate the load to failure of encapsulated posterior glass-ionomer (GI) restoratives tested under Hertzian indentation and to explore the validity and reproducibility of the test results achieved for consideration of inclusion as an ISO testing protocol. Methods Groups of 20 disc-shaped specimens (10.0±0.1mm diameter, 3.10±0.03mm thickness) were prepared (in batches of four) from three encapsulated posterior GI restoratives. Discs were tested while resting freely on a dentine analogue material at 24h under Hertzian indentation at a rate of 1mm/min delivered through a 20mm diameter hard steel ball. The failure mode and fracture origin of the GI specimens was assessed by fractography. Statistica…

MedWorm Sponsor Message: The blue sky scrub collection offers something for every medical professional. Offering some of the finest scrub clothing in the world.

MedWorm: Dentistry

Posted in Dental News.

Tagged with , , , , , , , , .